Udimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled Strips

Mianyang Baoheng New Material Technology Co.,Ltd
Contact Now

Udimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled Strips

  • 1
  • 2
  • 3

Brand Name : PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL

Model Number : Udimet 710, ATG W4

Certification : SGS, TUV, BV, ISO, MTC

Place of Origin : China

MOQ : 600kg

Price : Negotiations

Payment Terms : T/T

Supply Ability : 50000KGS/Month

Delivery Time : Ex-stock for delivery: 3-7 days Production lead time: 30-60 days

Packaging Details : Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement

Product Name : Udimet 710, ATG W4 Superalloy

Characteristic : Anti-oxidation, Creep resistance

Heat treatment condition : +P, +NT, etc

Processing methods : Machined, etc

Available Shapes : Steel plate, Sheet, Coil, etc

Surface : Rrough Turned, Centreless Ground, etc

Contact Now

Udimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled Strips



Product Information

Udimet 710 superalloy has good oxidation resistance and creep resistance, and can be strengthened by precipitation hardening, solution hardening and work hardening. They also function under high mechanical stress and high temperature and where high surface stability is required


Size Range

Round bar / Wire rod (Diameter): 1.0 mm to 500 mm
Square bar / Flat bar: 1.0 mm to 500 mm
Forging piece: Stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.
Heavy/middle plate via hot rolled: T3 - 1000 mm X W8 - 1000 mm X L800-12000 mm
Sheet steel via cold rolled: T5.0 - 8 mm X W5 - 1000 mm X L100 - 1000 mm
Steel strip via cold rolled: T0.3 - 8 mm X W10 - 1000 mm X L (or in coil form)
Length: Fixed length or random length or based on the customer's special requirement.


Chemical Composition and standard


Udimet 710

ATG W4

ASTM A959(2004)

JIS G4303(2005)


C(%): ≤0.07
Si(%): -
Mn(%): -
P(%)≤: -
S(%)≤: -
Cr(%):
≤18.0
Ni(%): ≤55.0
Mo(%): ≤3.0

W(%): ≤1.50

Al(%): ≤2.50

Ti(%): ≤5.0

Fe(%): ≤0.50

Co(%): ≤14.8

B(%): ≤0.02

C(%): ≤0.07
Si(%): -
Mn(%): -
P(%)≤: -
S(%)≤: -
Cr(%):
≤18.0
Ni(%): Remainder
Mo(%): ≤3.0

W(%): ≤1.50

Al(%): ≤2.50

Ti(%): ≤5.0

Fe(%): -

Co(%): -

B(%): ≤0.02


Udimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled Strips
X120Mn12/1.3401 Mechanical Properties

Tensile strength, Rm/MPa: -
Yield strength, Rp/MPa: -
Elongation/%: -
Reduction of area, ψ/%: --

Impact, KV /J: -
Hardness, HBW: --


Applications

Udimet 710 is suitable for various high-temperature environments, such as steam and gas turbines.

If you are interested in our products or have any questions, please contact our team of engineers at
sales@ss-bars.com


Udimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled StripsUdimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled Strips


Udimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled Strips


Product Tags:

Udimet 710 Superalloy Sheet Steel

      

ATG W4 Hot Rolled Strips

      

ASTM A959 Superalloy Sheet Steel

      
Cheap Udimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled Strips for sale

Udimet 710 Superalloy Sheet Steel ATG W4 Hot Rolled Strips Images