Sign In | Join Free | My insurersguide.com
China Mianyang Baoheng New Material Technology Co.,Ltd logo
Mianyang Baoheng New Material Technology Co.,Ltd
Quality Solutions. Trusted Partners.
Active Member

4 Years

Home > Steel Forging Parts >

Nimonic 80A Steel Forging Bar Superalloy Hot Forged Piece HEV5 NiFi25Cr20NbTi ESR

Mianyang Baoheng New Material Technology Co.,Ltd
Contact Now

Nimonic 80A Steel Forging Bar Superalloy Hot Forged Piece HEV5 NiFi25Cr20NbTi ESR

  • 1
  • 2
  • 3

Brand Name : ANSTEEL,TISCO,BAOSTEEL,PANGANGGROUP

Model Number : HEV5,Nimonic 80A,NiFi25Cr20NbTi

Certification : SGS,TUV,BV,ISO,MTC

Place of Origin : China

MOQ : 500kg

Price : 22000-25000 USD/Ton

Payment Terms : T/T

Supply Ability : 160000KGS/Month

Delivery Time : Ex-stock for delivery: 3-8 days Production lead time: 30-60 days

Packaging Details : Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement

Product Name : Nimonic 80A Superalloy Forging Piece

Executive Technical Standard : SAE,DIN EN,etc

Processing methods : sground, milled etc

Price Term : CIF, CFR,Ex-work, FOB, DDU

Contact Now

Nimonic 80A Superalloy Forging Piece HEV5 Forgings Hot forged NiFi25Cr20NbTi ESR

Description

Our company provides HEV5 Superalloy Forging Piece Nimonic 80A Forgings Hot forged NiFi25Cr20NbTi ESR SAE J775-1993

All of HEV5 Superalloy Forging Piece Nimonic 80A Forgings Hot forged NiFi25Cr20NbTi ESR SAE J775-1993 conform to Military standard, nuclear power. 100% Ultrasonic test

  • Material:Metal,Superalloy Forging Piece,HEV5,Nimonic 80A,NiFi25Cr20NbTi.
  • Executive Technical Standards: GB / ISO / DIN / NF / BV / BS / JIS / JASO / NDS / ASTM / SAE / UNS / AISI etc.
  • Metal Type:Superalloy series.
  • Shape:Superalloy Forging Piece.
  • Forging piece: stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.
  • Length: Fixed length or random length or based on the customer's special requirement.
  • Surface:Black,Bright or According To Customer Demand.
  • High Light:Superalloy Forging Piece,HEV5,Nimonic 80A,NiFi25Cr20NbTi.

Packing details:

Products are well packed and clear labeled according to the regulations and customer's requests.

Intact packages are able to avoid any damage which might otherwise be caused during storage or transportation.

Products Details

ASTM 8620H Structural Steel Forging Piece UNS H86200 Forgings 1.6523 ESR ASTM A304-2004

Chemical Composition (weight%): Mechanical Properties Under Final Heat Treatment:
C (%): ≤ 0.10
Si (%): ≤ 1.00
Mn (%): ≤ 1.00
P (%)≤: 0.020
S (%)≤: 0.015
Cr (%): 18.0 ~ 21.0
Ni (%): Balance
Ti (%): 1.80 ~ 2.70
Al (%): 1.00 ~ 1.80
Others (%): Co ≤2.00, Cu ≤0.20,Fe ≤3.00, B ≤0.008,Zr ≤0.15
Condition: heat treatment
Tensile strength, σb/MPa: 1130 Min.
Yield strength, σ0.2≥/MPa: 985
Elongation, δ5≥(%): 5.0
Reduction of area, ψ≥(%): -
Hardness ≥: -

Applications:

Driveshafts
Gears
Fasteners
Landing and takeoff gear
Missile and ejector systems
Torsion springs

Nimonic 80A Steel Forging Bar Superalloy Hot Forged Piece HEV5 NiFi25Cr20NbTi ESR

Technical Standard Equivalent Grade
DIN EN 10090(1998)

NiFi25Cr20NbTi

Nimonic 80A
SAE J775 HEV5

Nimonic 80A Steel Forging Bar Superalloy Hot Forged Piece HEV5 NiFi25Cr20NbTi ESRNimonic 80A Steel Forging Bar Superalloy Hot Forged Piece HEV5 NiFi25Cr20NbTi ESR

FAQ

Q: How do you control the quality?

A: We have professional inspectors to analyze the chemical composition of raw materials and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.


Q: Do you accept customization?


A: Yes. If you have special requirements for products or packaging, we can make them for you.


Q: Can you accept trial orders?


A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.


Q: How do I get samples?


A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.

Nimonic 80A Steel Forging Bar Superalloy Hot Forged Piece HEV5 NiFi25Cr20NbTi ESR


Product Tags:

NiFi25Cr20NbTi Steel Forging Bar

      

Nimonic 80A Steel Forging Bar

      

Nimonic 80A

      
Cheap Nimonic 80A Steel Forging Bar Superalloy Hot Forged Piece HEV5 NiFi25Cr20NbTi ESR for sale

Nimonic 80A Steel Forging Bar Superalloy Hot Forged Piece HEV5 NiFi25Cr20NbTi ESR Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Mianyang Baoheng New Material Technology Co.,Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)