Sign In | Join Free | My insurersguide.com
China Mianyang Baoheng New Material Technology Co.,Ltd logo
Mianyang Baoheng New Material Technology Co.,Ltd
Quality Solutions. Trusted Partners.
Active Member

4 Years

Home > Alloy Round Bar >

INCOLOY Alloy 800H Nickel Alloy Bar Superalloy Customized BV Standard

Mianyang Baoheng New Material Technology Co.,Ltd
Contact Now

INCOLOY Alloy 800H Nickel Alloy Bar Superalloy Customized BV Standard

  • 1
  • 2

Brand Name : PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL

Model Number : INCOLOY alloy 27-7Mo

Certification : SGS,TUV,BV,ISO,MTC

Place of Origin : China

MOQ : Negotiations

Price : Negotiations

Payment Terms : T/T

Supply Ability : 100000KGS/Month

Delivery Time : Ex-stock for delivery: 3-7 days Production lead time: 45-55days

Packaging Details : Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement

Product Name : INCOLOY alloy 800H Alloy Round Bar

Grades : INCOLOY alloy 800H

Processing methods : Shot blasted,Peeled,Cold working,Machined,etc

Surface : Black,Rrough Turned,Grinding,Centreless Ground,etc

Profile : Round Bar,,Forging Parts,Sheets Plates,Forging Piece,etc

Price Term : Ex-work,FOB,CIF, DDU etc.

Contact Now

INCOLOY alloy 800H Alloy Round Bar 800H Superalloy Round Bar 800H Round Bar 800H Bar

Description

Our company provides INCOLOY alloy 800H Alloy Round Bar 800H Superalloy Round Bar 800H Shot blasted Round Bar 800H Machined Bar.

All of INCOLOY alloy 800H Alloy Round Bar 800H Superalloy Round Bar 800H Shot blasted Round Bar 800H Machined Bar conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.

  • Material:Metal,INCOLOY alloy 800H Alloy Round Bar 800H Superalloy Round Bar 800H Round Bar 800H Bar
  • Shape:Superalloy Round Bar
  • Round bar / Wire rod (Diameter): 5.5mm to 800mm

  • Square bar / Flat bar: 3mm to 800mm

  • Forging piece: stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.

  • Heavy/middle plate via hot rolled: T6 - 200mm X W10 - 1500mm X L1000-12000mm

  • Sheet steel via cold rolled: T0.5 - 6mm X W6 - 1000mm X L1000 - 2000mm

  • Steel strip via cold rolled: T0.1 - 3mm X W5 - 200mm X L (or in coil form)

  • Length: Fixed length or random length or based on the customer's special requirement.

Products Details

INCOLOY alloy 800H Alloy Round Bar 800H Superalloy Round Bar 800H Shot blasted Round Bar 800H Machined Bar

Chemical Composition (weight%): Mechanical Properties Under Final Heat Treatment:

C (%): ≤ 0.08
Cr (%):≤ 21.0
Ni (%): ≤ 32.0
Al(%): ≤ 0.30
N (%): 0.30 ~ 0.40
Ti(%): ≤ 0.40

Fe(%): ≤ 45.5

Form: rod and bar
Condition: cold worked and hot worked, annealed, at 1121 Deg. min.
Tensile strength,σb/≥ MPa: 450
Yield strength, σ0.2/≥ MPa: 170
Elongation, δ ≥(%): 30.0
Reduction of area, ф ≥ (%): -
Hardness | HRC: -

Service temperature: above 593 Deg

INCOLOY Alloy 800H Nickel Alloy Bar Superalloy Customized BV Standard

Applications:

INCOLOY alloy 800H Alloy Round Bar 800H Superalloy Round Bar 800H Shot blasted Round Bar 800H Machined Bar

Superalloy is widely used to produce the high temperature components for gas turbine in the field of aviation, naval vessels and industry, such as turbine blade, guide blade, turbine disc, high pressure compressor disc, combustor, and also production of energy conversion devices, such as aerospace craft, rocket motor, nuclear reactor, petrochemical equipments, coaly transforming and so on.

INCOLOY Alloy 800H Nickel Alloy Bar Superalloy Customized BV StandardINCOLOY Alloy 800H Nickel Alloy Bar Superalloy Customized BV Standard

INCOLOY alloy 800H Alloy Round Bar 800H Superalloy Round Bar 800H Shot blasted Round Bar 800H Machined Bar

FAQ

Q: How do you control the quality?

A: We have professional inspectors to analyze the chemical composition of INCOLOY alloy 800H Alloy Round Bar 800H Superalloy Round Bar 800H Round Bar 800H Bar and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.


Q: Do you accept customization?


A: Yes. If you have special requirements for products or packaging, we can make them for you.


Q: Can you accept trial orders?


A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.


Q: How do I get samples?


A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.

INCOLOY Alloy 800H Nickel Alloy Bar Superalloy Customized BV Standard

Packing method

Wooden Pallet BOX,Standard Seaworthy Package,based on the customer's special requirement,etc


Product Tags:

customized nickel alloy bar

      

INCOLOY Alloy 800H nickel alloy bar

      

INCOLOY Alloy 800H

      
Cheap INCOLOY Alloy 800H Nickel Alloy Bar Superalloy Customized BV Standard for sale

INCOLOY Alloy 800H Nickel Alloy Bar Superalloy Customized BV Standard Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Mianyang Baoheng New Material Technology Co.,Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)